I need a hand and advise how to braze 1.5 mm galvenized wire
with a gas torch what type of feeling material to use? this
is for hobby use at home
thanks Danny Katz Israel
 
If you don't need a whole lot of strength (based on the wire size, you probably don't!) then soldering would be the most expedient means to connect the wire. It could be done with a low heat torch and is much easier to do properly than brazing.

Consider using a high tin solid solder with appropriate flux for the application.
 