Hi guys,
i had an inspection on a site where they were pouring a concrete Slab. The concrete is C35/45. The concrete slump is reaching 21 cm although no superplasticizer has been added to the mix. it is too much since the allowable for slabs as i know is around 14 cm.
What is weird is that the cube tests are giving very good results. The recommnended is 45 and they are reaching 55Mpa.
any ideas ?
i had an inspection on a site where they were pouring a concrete Slab. The concrete is C35/45. The concrete slump is reaching 21 cm although no superplasticizer has been added to the mix. it is too much since the allowable for slabs as i know is around 14 cm.
What is weird is that the cube tests are giving very good results. The recommnended is 45 and they are reaching 55Mpa.
any ideas ?