Can somebody please interpret/advise on the following from BS EN 15614-1 in particular the note underlined.
This is in relation to potentially using a PQR done with 141 root and pass(es) and 111 fill and cap to qualify a 141 process only WPS
Para 8.4.1 "For multi-process procedures the welding procedure qualification may be carried out with separate welding
procedure tests for each welding process. It is also possible to make the welding procedure test as a multi-process
procedure test. The qualification of such a test is only valid for the process sequence carried out during the multi process procedure test.
NOTE It is not allowed to use a multi-process procedure test to qualify any single process unless the testing carried out on
the process conforms to this standard."
Does this relate to Para 7.5.4 Impact Testing? "Where multiple welding processes are qualified in a single test piece, impact test specimens shall be taken from
the weld metal and HAZ that include each process."
Regards
Jason Symons
This is in relation to potentially using a PQR done with 141 root and pass(es) and 111 fill and cap to qualify a 141 process only WPS
Para 8.4.1 "For multi-process procedures the welding procedure qualification may be carried out with separate welding
procedure tests for each welding process. It is also possible to make the welding procedure test as a multi-process
procedure test. The qualification of such a test is only valid for the process sequence carried out during the multi process procedure test.
NOTE It is not allowed to use a multi-process procedure test to qualify any single process unless the testing carried out on
the process conforms to this standard."
Does this relate to Para 7.5.4 Impact Testing? "Where multiple welding processes are qualified in a single test piece, impact test specimens shall be taken from
the weld metal and HAZ that include each process."
Regards
Jason Symons