Jun 28, 2005 #1 Wyssbrod Mechanical Joined Jun 28, 2005 Messages 1 Location CH Hi, I'd like to make structural simulations with the material PMMA. What material properties or laws best describe the material behavior of PMMA under structural loads? Thanks.
Hi, I'd like to make structural simulations with the material PMMA. What material properties or laws best describe the material behavior of PMMA under structural loads? Thanks.
Jun 30, 2005 #2 dwightdixon Materials Joined Dec 15, 2004 Messages 130 Location US Get the physicals from the material suppliers. Nice thing about pmma is you can use polarized light to measure the stresses. Upvote 0 Downvote
Get the physicals from the material suppliers. Nice thing about pmma is you can use polarized light to measure the stresses.