Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Simulation of Tensile test coupon for large plastic deformation and stress triaxility correction

Status
Not open for further replies.

bedyhope

Mechanical
Joined
Sep 6, 2013
Messages
6
Location
MY
i am simulating tensile test coupon to get true stress-strain beyond necking through revers method or so called trail and error method using Abaqus. the problem am facing is that, when i run the simulation using standard solver the obtained force is very high compare to experimental one. however, when i use nonlinear geometry option (NLGEOM) in abaqus the the results seems good until the non-geometrical necking start where the global force will drop rapidly. i tried to solve this through necking effect correction but it does not work. any hint will be appreciated.
 
Perhaps you should incorporate *POROUS METAL PLASTICITY in order to simulate the softening due to micro-void development?
 
thank mrgoldthorpe

yes its an option that requires additional work to get model parameters for Gurson model. but the experimental load-displacement does not show any softening till the fracture point which correspond to localized necking. the weird thing here is that the load (from simulation) after elastic limit shoot a bit high compare to experimental results.
 