I am trying to get accustomed with STAAD and I started with simple plate 15 cm thick, dimension 5x5 m fixed on all four sides.
I used concrete for material (E=21700 N/mmsq, Poisson 0.17) and plate has quad division of 10x10.
Results I obtain above supports are not very similar with theoretical and results from another programs.
Moment above support is Mx=0.796 kNm/m what is significantly less than theoretical result (1.30 kNm/m). In AxisVM and SAP2000 I got 1.27 kNm/m
In the middle of plate I got Mx=-0.49kNm/m, which is more close to theoretical (-0.525).
What is wrong?
Thanks.
Version: STAAD Pro 2004, WIN2k
I used concrete for material (E=21700 N/mmsq, Poisson 0.17) and plate has quad division of 10x10.
Results I obtain above supports are not very similar with theoretical and results from another programs.
Moment above support is Mx=0.796 kNm/m what is significantly less than theoretical result (1.30 kNm/m). In AxisVM and SAP2000 I got 1.27 kNm/m
In the middle of plate I got Mx=-0.49kNm/m, which is more close to theoretical (-0.525).