We have a major problem with silicone contains glass fibers.
Till now we have done severals trials and non of them has given good results. Base on our results we know that in this case the properties of extruded parts (before curing) and exrtrusion itself depends on rubber viscosity. The temperatures of extruding is below 50C (as recommended by producer). The hoses after extrusion are so soft that it is impossible to put them on mandrelas. we tried to increase viscosity to sertain level but we decrease the scorch time simultaneously...
Pre-curing is just a temporary solution; not to implement for serial production.
if you have any experience with that kind of rubber/problem;please give me some tips. any help welcomed.
Till now we have done severals trials and non of them has given good results. Base on our results we know that in this case the properties of extruded parts (before curing) and exrtrusion itself depends on rubber viscosity. The temperatures of extruding is below 50C (as recommended by producer). The hoses after extrusion are so soft that it is impossible to put them on mandrelas. we tried to increase viscosity to sertain level but we decrease the scorch time simultaneously...
Pre-curing is just a temporary solution; not to implement for serial production.
if you have any experience with that kind of rubber/problem;please give me some tips. any help welcomed.