I once used a silicon carbide fiber over 1 meter.

Where to buy such fiber do you know?

 
Replies continue below

Recommended for you

Performance Composites Ltd in the UK have various fibres left over from some MMC research projects including

'Nicalon' silicon carbide fibre
Alumina fibre
Boron filaments woven with titanium.
P55 & P75 Carbon fibre.

contact email sms@performance-composites.com
 