shrinkage,

  • Thread starter Thread starter rmatija
  • Start date Start date
R

rmatija

Guest
Mmaterial:POM Hostaform C9021


Shrinkage in Mold design


Can sombsdi help


Thaks
 
You can check on data sheet and this could be find on website.
its 1.8% across flow direction and 2% in flow direction.
 