Doesn't a structural plain concrete foundation need reinforcement for shrinkage effect? I have gone through ACI-318, chapter 22 "Structural Plain Concrete" and found out no indication to such reinforcement. If such reinforcement is need, where shall it be placed?

Thanks and regards,



 
Replies continue below

Recommended for you

Reinforced concrete needs reinforcement, for shrinkage among a lot of other reasons. Plain concrete is unreinforced. You will find that the code has different rules for plain and reinforced concrete.
 