Dear All,

Why must all shop welded tanks' bottom plates be butt welded rather than lap welded as per J.3.1.5 11th Edition?

Thanks
 
Replies continue below

Recommended for you

Because of the high bending stresses in the bootm plate induced by the shop air test.

Joe Tank
 