Shock absorbents; heat dissipation

Status
Not open for further replies.

Shabaa

Electrical
Joined
Jan 6, 2005
Messages
1
Location
CA
I am wondering what are some of the most effective materials for sealing sensitive electronics against shock, and vibrations. Also, it is important that the materials can dissipate heat readily. Any ideas?
 
Hi Shabaa,

We have successfully used in the past SMACTANE material:


However, the requirements for a shock or vibration isolator/damper material might be incompatible. Really think about from what kind of excitations you want to protect your equipment.

I think we used Viton Material as well.