QualityAsia
Structural
- Apr 7, 2009
- 11
MY Owner has been requesting me to specify 99.997% Argon gas composition in our revised WPS, questions as below,
1. Are there any papers to support minimum 99.997% Argon gas composition required for GTAW?
2. 99.9% Argon gas composition was specified in old PQR. Can I specify 99.997% Argon gas composition in new WPS?
3. How many percents of Argon gas composition generally were used for offshore and onshore weldings by GTAW process.
Thanks & Regards
QualityAsia
1. Are there any papers to support minimum 99.997% Argon gas composition required for GTAW?
2. 99.9% Argon gas composition was specified in old PQR. Can I specify 99.997% Argon gas composition in new WPS?
3. How many percents of Argon gas composition generally were used for offshore and onshore weldings by GTAW process.
Thanks & Regards
QualityAsia