Mar 18, 2004 #1 Terry Mechanical Joined Feb 20, 2001 Messages 1 Location US is it possible to bend up two adjacent sides of a sheet metal box using a press brake and have them meet at the corner?
is it possible to bend up two adjacent sides of a sheet metal box using a press brake and have them meet at the corner?
Mar 19, 2004 #2 deanc Specifier/Regulator Joined Sep 18, 2002 Messages 855 Location US Of course. Segmental top dies. May need to be long. A cheat is to fold out the corners and reposition them when you are finished. Brake at the end of the dies so you only have two corners to reform. Make sense? Upvote 0 Downvote