112275
Marine/Ocean
- Jan 8, 2003
- 58
I need to form a 1" flange along a curved edge of 10 gauge aluminun 5052-h34. curve would be aprox 48" long with a 6 foot radius. What type of machine would do this. also i would want the part to also be resonably flat
thanks