Hi ,

I am using a shear pin for stem protection
at maximum torque. See picture attached.

How to calculate shear pin failure before stem failure?

Following are the inputs I have,

dia of shear pin,d = .625 in
dia of stem ,D = 1.5 in
Max Torque ,T = 3250 in.lbf
UTS of shear pin = 58000 psi
Yield strength of shear pin = 36000 psi

Thanks !


 
 https://files.engineering.com/getfile.aspx?folder=6a224695-7ec8-4dda-bf5c-ce79950de96d&file=96A327F0-EAFB-431C-88BB-B4063BC36D00.gif
Pull out your favorite strength of materials reference and look up double shear.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
All shear and no bending calc's if the diagram is correct.
 