drscottuk

Structural
Joined
Jun 21, 2007
Messages
23
Location
GB
I'm trying to scour for some way of calculating the shear capacity of 304L stainless steel sheet. BS5950 doesn't cover it, neither does the BSSA (british stainless steel assoc), or the SCI. I have read through any relevant publication I can find on their sites.

I have checked through tables of the larger stainless suppliers like Eurosteel but they dont give shear capacity for thin sheet either. There must be some way to calc it?

I saw a previous similar thread for a different grade stainless steel, where this relationship relationship was used:

? = 0.6 · ?

where

? is the shear strength
? is the tensile strength

In the previous post it was mentioned austenitic materials have different strain hardening properties than the formula above. Is there any literature I can find a formula for austenitic steel? Any advice is appreciated!
 
hmm for some reason the forum cant display tau and sigma symbols. The formula above is this:

shear strength = 0.6 * tensile strength
 
I can't help you technically but you can put the equation as below.

[τ] = 0.6*[σ]

Code:
[τ] = 0.6*[σ]

Go to the Process TGML and follow the code for Greek letters.

 
You can use the formula above for your work.

The basis for this formula is the von Mises/Huber/distortion energy failure criterion. This states that yielding in shear occurs at a stress level that is equal to 0.577 times the tensile yield stress.

Due to the variation in strain hardening between slip systems, the natural spread in fracture strength and elongation for a material, and to avoid using more significant digits than are warranted, the 0.577 factor becomes 0.6.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
If you are looking at ultimate shear strength and ultimate tensile strength values for austenitic stainless steel, an excellent source of tabulated values is below from the US Department of Defense, and can be downloaded from the Internet;

Military Handbook
MIL-HDBK-5H

 