Greetings,
I've got a couple of old, relatively small castings of a material that I can't identify other than to categorize them as white metal--almost certainly a zinc alloy.
I'm planning to utilize self-tapping screws as I modify the castings for reassembly. My question is:
What is the ideal self-tapping screw tip configuration for this type of material? I've considered a Type BT (25), Type BF and a Type T (23), but would value inputs.

Thanks in advance.

Paul
 
Thanks, gents. I'll give them a look.

Paul
 
I would second Cory. Taptite or Delta PT. it should be a simple application if you have enough length of engagement.
 