courtl
Aerospace
- Feb 18, 2002
- 23
Hi,
I am looking for a fairly quick setting, low temp cure potting compound or epoxy/adhesive that is self levelling/low viscosity. It will be used to fill fairly wide/long (only 1 -2mm deep) voids in a PCB. It also needs to be non-conductive. It doesn't have to set hard, so can be rubbery. Can anyone suggest anything?
Thanks in advance,
Linda
I am looking for a fairly quick setting, low temp cure potting compound or epoxy/adhesive that is self levelling/low viscosity. It will be used to fill fairly wide/long (only 1 -2mm deep) voids in a PCB. It also needs to be non-conductive. It doesn't have to set hard, so can be rubbery. Can anyone suggest anything?
Thanks in advance,
Linda