Dear Friends
I need your help in understanding AWS D1.1-2008 Table 3.1-Note 1 which provide Options in selecting right consumable
1)Filler metal matches higher strength of base material
2)Filler metal matches lower strength of base material
I need to weld Group I - Mat Grade D x Group Material Grade EH36. Weld Process - SMAW.
What would the be right electrode - E7016 or E7018?
Thanks
I need your help in understanding AWS D1.1-2008 Table 3.1-Note 1 which provide Options in selecting right consumable
1)Filler metal matches higher strength of base material
2)Filler metal matches lower strength of base material
I need to weld Group I - Mat Grade D x Group Material Grade EH36. Weld Process - SMAW.
What would the be right electrode - E7016 or E7018?
Thanks