Hi all,
I am developing a product and need a source for 2.5mm wire coated with volumetrically conductive plastic for use within a concrete wall.
The reason I desire this material is that it is not subject to corrosion as would be standard wire when imbedded in a damp concrete wall.
Any assistance is greatly appreciated.
Regards,
Jon
 
Replies continue below

Recommended for you

It might end up more expensive than stainless steel wire.

How much do you need.

I can put you in contact with a source of conductive plastic suitable for cable coating, and possibly in contact with a cable or wire coater.

Cable or wire coating machines normally run very fast, so nthere is a lot of wastage on start up, therefore short runs are difficult, or at least expensive.

Regards
pat pprimmer@acay.com.au
eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor