Any help about possible usage (or disposal options) for lead slag?
it has 55% of Fe and 1.5% of Pb. It is obviously a dangeours residue, so disposal is both expensive and complex.
Any suggestion is welcomed.
Thnks
Pablo
 
Replies continue below

Recommended for you

Hi Pabasolo,

I work in a secondary lead plant in Australia, and would be interested in comparing notes with you.. Currently we send our secondary lead slag to prescribed waste but are researching alternatives.

Kind regards,
Chris James