hello
recently we have upgraded mechanical seal on a wax feed pump from API plan 02/62 to 02/53B/61 after 3 days we have faced leakage of barrier fluid on the outboard seal almost we top up frequency is almost every 3 hours. after opening we have discovered cock on the atmospherique side of the seal.
but all process data are within the limit , we have not see any rise on the barrier temeprature , we have well vented the loop during commissioning , cooling water also is fine we do not understand how it happen ? any suggestion
recently we have upgraded mechanical seal on a wax feed pump from API plan 02/62 to 02/53B/61 after 3 days we have faced leakage of barrier fluid on the outboard seal almost we top up frequency is almost every 3 hours. after opening we have discovered cock on the atmospherique side of the seal.
but all process data are within the limit , we have not see any rise on the barrier temeprature , we have well vented the loop during commissioning , cooling water also is fine we do not understand how it happen ? any suggestion