If I am flowing Argon inside my solenoid valve, would I be needing Viton seals? Would Buna N work?
Thanks!
 
Replies continue below

Recommended for you

Buna N should work fine. SBR ("Buna") rubber maybe a little more leak-tight. The only reason to use Viton is if you think your Argon is corrosive, which is unlikely since it's one of the noble gases, and hence very very un-reactive chemically.
 
You should consider the pressures! I assume they are low because if you are operating at high pressures you may experience explosive decompression.

trust this helps.
 