hi all, i'm mechanical engineer at bp operation in tangguh LNG, papua. i wanna ask a question about sea water intake line material, is it safe if we are using the GRE pipe,or I should use a super duplex material, and does anybody has an information about the price of super duplex material, thx

Bilal Adi Akbar
Mechanical Engineering Challenger
BP Tangguh Operation
 
You have posted this question in the wrong forum. Post it in Pipelines, Piping and Fluid Mechanics and you will get a better response.

Having said that ... What would be unsafe about GRE for this service ? It's commonly used fro raw seawater.
 