I need to attach an aluminum track overhead to a structural steel tube header.
I need to use #12-24 machine screws
What material should I use (and what materials to avoid)?
This is for folding (exterior) doors, hung from above and guided in a track below. Vertical support is at the top tract only.
I've been told to use 316 stainless. I'm hoping that is right but I'm concerned about the SS threads inside the carbon steel tube - 5/8 wall thickness will be drilled and tapped. Can't get thread rolling screws in the size I need 12-24 x 3.5" long)
Does all this sound correct?
Would zinc coated carbon steel be "better"?
Thanks
I need to use #12-24 machine screws
What material should I use (and what materials to avoid)?
This is for folding (exterior) doors, hung from above and guided in a track below. Vertical support is at the top tract only.
I've been told to use 316 stainless. I'm hoping that is right but I'm concerned about the SS threads inside the carbon steel tube - 5/8 wall thickness will be drilled and tapped. Can't get thread rolling screws in the size I need 12-24 x 3.5" long)
Does all this sound correct?
Would zinc coated carbon steel be "better"?
Thanks