Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

SCC of 17-4PH H900 Drive Rod 1

Status
Not open for further replies.

SSMroz

Materials
Joined
Dec 15, 2005
Messages
2
Location
US
I am currently working on a 17-4PH H900 drive rod that failed by SCC. I am having troubles nailing down the possiable causes of SCC in 17-4PH. We have found traces of cholrine and sulfur in the corrosion products. The rod would have operated at temperatures up to 300-F. Are cholrin or sulfur known to cause SCC at these temperatures? Also, pits were observed along the surface that the SCC intiated.

Thanks for any help anyone can offer.
 
YES.
If you have pits then you have active corrosion. Once that happens CSCC will be a high prob.
One problem with PH grades in there highest strength condition is that the CSCC easily.

= = = = = = = = = = = = = = = = = = = =
Corrosion, every where, all the time.
Manage it or it will manage you.
 
Thank-you all for the resources. They were very helpfull in this situation.

 
The docuement located at the NASA link I supplied above is already out of date. MSFC-STD-3029 (not "MSFC-SPEC-3029" as I typed above), is currently at the "A" revision...
 