Hi, im writing from venezuela.
I need to know how is posibble that im having scaling in my evaporative condenser if my water feed is:
TDS: 320 ppm
Total Hardness: <10 ppm
pH: 7.2
bicarbonates: 190 ppm
Silice: 29 ppm.
Temp: 77 F.
i work the condenser at 4 cycles max.:
in the basin have:
TDS: <1300 ppm
Total Hardness: <50 ppm caco3
pH: < 9.1
bicarbonates: <800 ppm caco3
Silice: <120 ppm.
Carbonates: <100 ppm caco3
the residual of ortophosfathes is near to 12 ppm. and the dispersant its near of 24 ppm. (continue dosification) and the critic temperature is near to 95 Fahrenheit.
Thanks.
I need to know how is posibble that im having scaling in my evaporative condenser if my water feed is:
TDS: 320 ppm
Total Hardness: <10 ppm
pH: 7.2
bicarbonates: 190 ppm
Silice: 29 ppm.
Temp: 77 F.
i work the condenser at 4 cycles max.:
in the basin have:
TDS: <1300 ppm
Total Hardness: <50 ppm caco3
pH: < 9.1
bicarbonates: <800 ppm caco3
Silice: <120 ppm.
Carbonates: <100 ppm caco3
the residual of ortophosfathes is near to 12 ppm. and the dispersant its near of 24 ppm. (continue dosification) and the critic temperature is near to 95 Fahrenheit.
Thanks.