Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Scale accumulation and Filtration 1

Status
Not open for further replies.

nornrich

Mechanical
Joined
Jun 12, 2002
Messages
194
Location
US
All,

In the plant I am working we are having a problem with our quench water distribution system. The system was orginally designed with little to no carbon scale byproduct in the process. Now there is carbon scale being generated and it is getting into the water circulation system for the process cooling water. Does anyone know of the best method for filtering this out of the system.

Regards,

Rich....[viking]

Richard Nornhold, PE
ampdesign@earthlink.net
 
As there is no flow rates given I’ll start with these people. We have several cooling systems that generate undesirable solids in their systems and we use both full stream and side stream strainers filters to kept the particulate material under control.


We have one system where there is a particular sticky monomer in cooling and scrubbing loop and we use this type filer. This might be the way to go as you mention build up.


Another type used is.


If you could comeback with a little more information about you system it would be helpful in getting you on the right track on whether you need a strainer or filter and what type.
 
Unclesyd,

The main circulation loop is 300GPM and the drops that feed the quench equipment are 60 GPM. The scale is being generated by the quench equipment. I would like to filter in the main loop and not at each piece of equipment.

Regards,

Rich....