X6CrNiTi18-10 material is listed under ASME IX as P8 Gr.1 material. But specification (SA/EN10028-7) that is listed is for flat products only. If we have to weld a pipe of this very same material then would it be considered as P8 or unassigned material ?
 
Pipe would be to I think EN 10216-5/-7, depending on long seam type.
If this standard isnt in your code section (like ASME II-D or IX), then its unassigned.
 