SA-705 pressure vessel

Status
Not open for further replies.

metalonis

Mechanical
Feb 28, 2002
183
ASME SA-705 Type 630 condition H1150 list strengths for forgings up to 8 inches in diameter. Does this mean that vessels larger in diameter are not permitted?
 
Replies continue below

Recommended for you

You have confused Applicable Thickness (of the base metal forging) in Table 3 with diameter.
 
The forging is a solid bar, not a forged shape.
 
But it will be drilled out. Final heat treatment will be after drilling out.
 
Typically we would take a solid cylindrical heat-treated forging and then machine the bore and closure. Heat treatment after machining looks like a possible option. Thanks for the idea.
 