Hi
Can I use SA 420 WPL6 for temp -20F to 250F to replace SA234 WPB in ASME VIII Div 1?. Because SA420 specify as Low Service Material?.
 
Replies continue below

Recommended for you

Yes you can for your stated service conditions. ASME SA-420 is endorsed by Section VIII, Div 1 for use up to 850 deg F. See Section II, Part D. The allowable stresses for WPL6 and WPB are equal at 250 deg F and below.
 