Hi guys,
I found some conflicting information in the thread #177-44286.
Can anyone, who is in posession of pre 1962 ASME check for me the allowable stress value for SA-212 B in room temperature?
Thank you kindly.

Putting Human Factor Back in Engineering
 
Replies continue below

Recommended for you

For SA-212-B, the allowable stress is 17.5 ksi all the way up to 650°F.

-Christine
 
Thanks, Christine.