Basically the title is my question. I cant find the UNS equivalent to these two materials S420 Structural Steel and Strenx® 700 Structural steel
I need to find the UNS equivalents for those two materials in ASME II Part D. Any help would be appreciated
BR, Sergey
 
Replies continue below

Recommended for you

Contact the owners of the linked websites for information.

Link
Link
 