we are storing galvanized steel chassis in a non air conditioned warehouse. I am located in Houston , Texas so the temps and humidity get VERY high. My question is , at what temp does rust begin ? what out of bounds limit should i set ?

any information is appreciated.

Thank you -
 
If the steel is galvanized, there should not be corrosion problems during short term storage, even in hot and humid environments. I recommend you visit the following website


There are good resources and background information on galvanizing.
 