Good Afternoon,
We are making several crossings under a few highways.
The highways are dual carriageway so quite wide.
The pipelines are carrying potable water in ductile iron cement-lined material from 800mm to 1600mm.
Is it normal to change the pipe material to HDPE and use a steel casing?
As the ductile iron is buried, up to the crossing area we are using the push-fit spigot socket joints. So could the DI pipe be flanged under the roads?
Any advice appreciated and whether there are any preferred methods of doing this in accordance with AWWA etc.
Best Regards
John
We are making several crossings under a few highways.
The highways are dual carriageway so quite wide.
The pipelines are carrying potable water in ductile iron cement-lined material from 800mm to 1600mm.
Is it normal to change the pipe material to HDPE and use a steel casing?
As the ductile iron is buried, up to the crossing area we are using the push-fit spigot socket joints. So could the DI pipe be flanged under the roads?
Any advice appreciated and whether there are any preferred methods of doing this in accordance with AWWA etc.
Best Regards
John