Anyone seen this before? Typically the radius is 0.8mm in acc with ASME B16.5
Requirement:
Ring type joint in high pressure and elevated temperature environments. The bottom groove radius shall be 3mm minimum
Reasoning:
Leakage from ring joint flanges in these services has occurred due to cracking emanating from the bottom groove radius - this is typically only 0.8mm and stresses imposed on such a sharp radius causes increased stress intensity which can crack under imposed mechanical and thermal loads.
Requirement:
Ring type joint in high pressure and elevated temperature environments. The bottom groove radius shall be 3mm minimum
Reasoning:
Leakage from ring joint flanges in these services has occurred due to cracking emanating from the bottom groove radius - this is typically only 0.8mm and stresses imposed on such a sharp radius causes increased stress intensity which can crack under imposed mechanical and thermal loads.