Apr 24, 2006 #1 dadfap Petroleum Joined Feb 1, 2003 Messages 72 Location NL Does anyone have a graphical representation of the Rockwell scale, showing differing metals and sand? Thanks dadfap
Does anyone have a graphical representation of the Rockwell scale, showing differing metals and sand? Thanks dadfap
Apr 24, 2006 #2 swall Materials Joined Sep 30, 2003 Messages 2,767 Location US If you can find a copy of "Elements of Materials Science" by Van Black, you will find just what you need in Appendix C. Upvote 0 Downvote
If you can find a copy of "Elements of Materials Science" by Van Black, you will find just what you need in Appendix C.