I need to have some rock privately tested ASAP.
I think we might have hit serpentine rock which you all know contains asbestos.
I need this done ASAP, I need to know procedures for transporting this material and if anyone knows of any geology labs in or around Manhattan that might be able to assist me..
Thanks
Joe
Project Engineer
I think we might have hit serpentine rock which you all know contains asbestos.
I need this done ASAP, I need to know procedures for transporting this material and if anyone knows of any geology labs in or around Manhattan that might be able to assist me..
Thanks
Joe
Project Engineer