Thank you in advance to any tips and advice.
My company is currently working on getting production up and running with a Capital Robotics Fusion Arc 180. Our current objective is to perform a consistent outside weld on a piece of stitch cut 14 ga sheet metal folded into a piece of angle. These parts are intended to be mass produced and this type of weld will be replicated on many of our future products. The weld is defective and has many blowholes and splatter throughout it after initial success earlier in the weld. Attached are the images of both a successful weld we are trying to imitate performed by our machine and one of their engineer representatives. The other images are obvious and very typical failures we're experiencing during testing.
Any help is greatly appreciated.
20191126_095552_g1avxo.jpg
20191126_095555_dmj1ln.jpg
20191126_095543_xktloe.jpg
 
Parameters and travel speed please?
What shielding gas do you use (+ flow rate)?
How is the surface prepared?
 
It is very unrealistic to expect robot troubleshooting advice or welding development from an online forum.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 