Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

retest and verification of raw material by vessel manufacturer

Status
Not open for further replies.

YuJie_PV

Mechanical
Jan 19, 2017
152
Fellew engineers, there is always a question wandering in my head. it is a general question that, as for ASME/EN code, in which occasion, shall the raw material (plate, forgings, etc) be mandated with retest and verification to be performed by vessel manufacturer? i mean chemical analysis, tensile test, and CVN test,etc to be performed.
Please shed some light on this topic, appreciate.
Thanks in advance.
 
Replies continue below

Recommended for you

Only when the original mark was not clearly transferred and traceability is in question.

Regards
 
Or perhaps you suspect counterfeit material...

Regards

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
I have seen it required, but it isn't common at all.
Usually if the service is that critical there was source inspection at the mill and the inspectors marks are clear on the paperwork and metal.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
You need to put it separately in the purchase order, but that would lead to an in increase in the cost!

DHURJATI SEN
Kolkata, India


 