Residual Magnetism for seamless pipe

Status
Not open for further replies.

zebmahar

Materials
Dec 12, 2010
46
Kindly tell me what is the requirement of residual magnetism for seamless pipe in API 5L 44th edition


Regards
Zebmahar
 
Replies continue below

Recommended for you

Short answer: Average of four circumferencial readings <30 Gs; no single reading > 35 Gs.

...You should get a complete copy for your use...See section E.7...the above is a brief paraphrase...
 