I am working on an asphalt repair/replacement project where we need to replace about 19,000 SY of asphalt between airfield shoulders and non-heavy equipment parking. The asphalt shows moderate alligator cracks however the asphalt is not under heavy use and is at least 10 years old. I suspect that much of the cracking is from aging as the location is southern california where the temperatures in the summer reach above 95F regularly. I am wondering if full base and subbase course replacement is really necessary or if removal of the asphalt and scarifying and recompacting the base course would be enough. Any suggestions for repair options that I may not have thought about?