I'm looking for a replacement for Durez 31906 Black phenolic. My problem is the lack of dimensional stability, and wear resistance after molding - both of which I have to improve. I'm willing to look at other phenolics, or even other MATERIALS all together.

Thanks for any suggestions!
 
can you give any more information about this part?
what kind of dimensional stability do you need and under what conditions-humidity, temperature?
what kind of wear?
thanks
 
It is a "flat" base plate that acts as a wear pad for a machine that operates (slides) mainly on wood. Flatness is the most important characteristic, followed by various concentricity call-outs. The warping, and shrinkage is not being controlled by the molder. I realize that the molder's processing is partly to blame, but I know that there is a better material out there to achieve my needs.

Temperature is not a factor (the sliding action on this plate is at a very low velocity). Humidity can be an issue, but this part is not being loaded funtionally.

Thanks
 
If this is a one-time part would you think of having the piece machined?
Unfortunately if the plate is not supported correctly, under humidity and temperature variations, the plate will deform. How about a plastic top screwed into a metal back plate? Then you dont have to worry about warpage.
Or if you could take the molded part and have it "finish" machined. Take it to a machine shop and have them do some surfacing to square the planes.

Good Luck.
 
hrvat, a helpful website is you can find material data, process guidelines, mold and part design tips. Also, you might want to investigate castable high hardness Polyurethanes ... 75 to 85 Shore-D Hardness. This
material offers high wear resistance & high load bearing strength. Tooling cost for building open cast molds are very low. There are numerous suppliers out there that will do a turn-key job for you
 