Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Remove wax from hot water or mineral oil. 3D Printer support material removal. 2

Status
Not open for further replies.

VeryFungi

Electrical
Joined
Feb 25, 2013
Messages
11
Location
US
Hi all,

I have purchased a 3D Systems ProJet 3500HD Max. After a very long ordeal I am finally making parts. I am trying to speed up and streamline the cleaning process. The short question is what is the easiest way to remove wax from 70c water in a continuous operation. In other words I do not want to cool the water to remove the wax. This is a very small operation.

I can make about 75 parts at a time, and they are about 1" x 1" x .5". The parts are UV cured acrylic and are completely encased in wax when they come off the printer. The parts can not withstand higher temperatures then 70c. The wax melts around 60c.

Here is the longer version. The parts come out of the oven 70c with a fair amount of wax remaining. The current process is to remove the parts one at a time and pat them down with a paper towel to soak up the wax. It doesn't get much before the wax cools.

Step two is a quick soak in heated 70c mineral oil, either in an ultrasonic cleaner, or a crock-pot. I have been able to sift off the top remaining wax on top of the cooled oil, but it is messy, I lose oil, and it doesn't get it all. I have tried a water based EZ-Rinse, but it get's saturated fast and the wax doesn't congeal very well on top of it. It's probably expensive.

The next step is to wash the parts in hot soapy water, I have to throw the water outside due to the oil in the water.

So far my only successes have been dying the parts black with RIT dye. A full container in about a gallon of water. This works very well, but any oil and wax left over saturates the top of the water inside the dying pot. Just pull the parts out of the dye through the junk you are trying to get rid of and it creates a thin film on the parts. Cleaning by hand can help remove some of this.

The final step is to seal the parts. I have so far not been able to get standard spray can paint or primer to cure properly. I'm assuming I have not removed the wax completely. I have considered a week sodium hydroxide wash, but am not crazy about it. I have had some success with painting with polyurethane. For now I'm doing it by hand by thinning water based Varathane 50% and brushing it on. I plan to spray it on eventually.

So I would like to replace all of this time consuming part by part handling. I would like to replace all of these steps excluding sealing with one operation. If the parts can be put inside a 70c water bath, but with circulation and filtering to remove the wax I think I could seal them directly.

I'm an Electronics Engineer so this is all alien to me. lol Please help me! :D
 
Interesting thread. I'm trying to get a 3D printer at work. All the various systems barely mention the work required to remove support material. From 3DSystems:

"VisiJet® S300 Support Material is used in the ProJet HD 3500, ProJet SD 3500, ProJet DP 3500, ProJet MP 3500 and ProJet 5000 Printers. It provides for hands-free, melt-away removal from even the most inaccessible geometry features and internal spaces with no damage to the most delicate part features."

Sounds like it practically removes itself. I'll have to be sure to pay more attention to this aspect when we select a system.

----------------------------------------

The Help for this program was created in Windows Help format, which depends on a feature that isn't included in this version of Windows.
 
dgallup said:
Interesting thread. I'm trying to get a 3D printer at work. All the various systems barely mention the work required to remove support material. From 3DSystems:

"VisiJet® S300 Support Material is used in the ProJet HD 3500, ProJet SD 3500, ProJet DP 3500, ProJet MP 3500 and ProJet 5000 Printers. It provides for hands-free, melt-away removal from even the most inaccessible geometry features and internal spaces with no damage to the most delicate part features."

Sounds like it practically removes itself. I'll have to be sure to pay more attention to this aspect when we select a system.

I'm also in search of a 3D printer for my company and we had the 3D systems rep visit to talk about the HD3500. The parts the rep brought looked great, and he claimed his cleaning method was simple: melt the wax off in an oven for a few hours, then clean any residual wax off with the ultra sonic cleaner. Now that I have seen this thread, I am skeptical about the simplicity of the process. It sounds like additional work is needed to get good, clean parts. I do like the fact the wax is essentially paraffin wax and supposedly non-toxic. Makes me feel better about throwing in the trash.
 
There is a new forum on this site, just created for 3D printing and manufacturing. It may not help you this time since it is empty, but if there is more activity it may be a good place to look for help. You could ask the moderator of this forum to relocate this thread, if you wanted to.
 