acrylonitrile
Chemical
Problem:A carbon steel distillation column'spot has a stainless steel (304L) liner (1/16") to protect the pot from Acedic acid corrosion.The liner was plug welded to the carbon steel shell of the pot. The problem is some of liner have been broken off from the shell and flamable materials have been got to the space between the liner and the shell.
What technique I can use to remove the liner? Are there any contractor that do this kind of services?
What technique I can use to remove the liner? Are there any contractor that do this kind of services?