Removal of 3 Layer Polyethylene on pipeline under water

Status
Not open for further replies.

NATIVES

Petroleum
Joined
Dec 5, 2010
Messages
16
Location
US
What is the ramification of removing 3 Layer Polyethylene on pipeline under water (offshore) to accommodate AUT inspection? Is it a common practice? Must the coating be removed to perform AUT inspection?
 
The pipe is much more likely to corrode?

What AUT are you doing?

Most UT I know will account for the thickness of the external coating.

This sounds very odd to me. How are you raising the pipeline off the seabed?

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Suppose you are carrying out AUT on overhead insulated piping. You remove the insulation, then do the AUT.
Same logic.

DHURJATI SEN


 
I wouldn't say that it is a common practice to deliberately damage the primary barrier to corrosion, particularly if the line can take ILI. It will be an expensive measure as the stuff doesn't come off easily.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Also "AUT" covers a multitude f different systems.

What and why are you doing it?

dhurjati - I don't agree this is the same thing.

3LPE is not designed to be removed and looses most is not all of it's properties of you do. Plus there should be no need.

What does the inspection company say?

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 