Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

relative stress relief condition - steel shaft material

Status
Not open for further replies.

Tmoose

Mechanical
Joined
Apr 12, 2003
Messages
5,636
Location
US
We make some steel shafts 9 to 12 inch diameter, up to 100 inches or so between bearings. A single row of Several 1 inch keyways are cut ~ inline along one side.
Historically a few shaft have reportedly "bent" in service. It is unclear if the shafts were straightened or needed straightening during manufacturing process.

Physical properties are satisfied with normalized or HR or annealed materials.

Which condition(s) is certain to resist distortion when asymetrically machined, as with a row of keyways?