Dear all,
When we transfer the temperature from heat transfer analysis to displacement/stress analysis(Sequential) in Abaqus, Can we transfer the elemental temperature, or only nodal temperature is possible? if yes
1.How can we transfer the elemental temperature(TEMP) in sequential analysis?
2.Is it possible to transfer the fraction of phase transformation calculated using USDFLD Heat transfer analysis to the stress/displacement analysis?
 
In sequentially coupled thermal stress analyses temperatures read into the stress analysis as predefined field are always nodal values. Then they are interpolated within elements.
 