Is there information available showing the radii for A36 structural angle?
 
I've seen "2x wall thickness" tossed around for outside radius on square tube, and "1x thickness" for the corner fillet on angle. Although I think it does (and is allowed to) vary by manufacturer and/or phase of the moon.
 